Basic Info

Model No.:  hengruitong

Product Description

Model NO.: hengruitong Application: Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project Material: LDPE Thicnkess: 0.1- 3 Mm Length: as Request Trademark: RUNTONG Origin: Dezhou, China Certification: CE, ISO Feature: Puncture Resistance, Impact Resistance, Tear Resistance Color: Black Width: 2- 6 M Function: Seperation, Waterproof, Antiseep Specification: 0.5- 3 mm HS Code: 39219090 Excellent waterproof material for foundabtion work of dams and ponds
Application:

1, Prevent leakage disposal in landfill or waste water or waste dregs disposing field.
2, River bank, lake dam, mine remainings, reservoir, tunnel. Liquid storage pool(pit, mine)
3, Preventing leakage in subway, basement, tunnel, hole. Anti-salt leskage in roadbed and other groundsill.
4, The plane direction laying of dam, the vertical direction laying for groundsill, used in the construction fence and waste material field.
5, Used in seawater of freshwater feed field
6, Used in groundsill of road, highway, railway and waterproof layer of swelling clay and wet collapsed loess.
7, Preventing leakage on rooftop
Black HDPE Plastic Sheet HDPE Geomembrane Factory
Black HDPE Plastic Sheet HDPE Geomembrane FactoryAquaculture:

Using the Geomembrane anti-seepage feature;
Geomembrane liners can be used as fish ponds, shrimp pond, and other aquaculture.

Landfill:

HDPE Geomembrane is the most widely used in landfill anti-seepage engineering material,
The use of main parts of the bottom of the landfill liner, landfill sealing cover, leachate regulating pool liner, etc.
HDPE geomembrane structure with smooth surface and textured surface, suitable for different sites.

Water Treatment System:

Geomembrane is applied to the adjustment of the power plant and sewage treatment plants pool;
And a series of water treatment systems.

Mining:

Geomembrane suitable mining: Washing pool, pool heap leaching, heap yard, dissolving tank, tank,
Storage area, the bottom line of the tailings seepage control, etc

Geomembrane Catergory:

Geomembrane including LDPE, LLDPE geomembrane, HDPE geomembrane, EVA geomembrane, ECB geomembrane, PVC Geomembrane geomembrane with textured surface.

FAQ
1. How about the delivery time?
Lead time since receipt of 30% T/T deposit payment: 3 weeks.
(Samples will be prepared within 3 days. )
2. What kind of payments does jenor support?
T/T, L/C, Cash are accepted.
3. What's are the MOQ?
Generally speaking, the MOQ is one container, but we can provide you samples for quality inspection.
4. Do you charge for the samples?
Accordeing to our company policy, the samples are freee, we only charge the freight fee. And we will return the freight fee during the next order.
5. Can you produce according to customers' design?
Sure, we are professional manufacturer, OEM and ODM are both welcome.
6. Can you tell me your main customers?
That's our customers' privacy, we should protect their information.
At the same time, please rest assured that your information is also safe here.
Thank you for your visiting!
Our Service
Other products:
Polypropylene biaxial geogrid , plastic mesh grid, Polyester Geogrid, Fiberglass Geogrid, polypropylene staple fiber needle punched non-woven geotextile felt, Polypropylene non-woven fabric for road, non woven geotextile felt, pp Non Woven Geotextile, pet non Woven Geotextile, short fiber non Woven geotextile , HDPE geomembrane, LDPE Geomembrane, geocomposite geogrid, Composite geomembrane, biaxial geogrid suppliers
LDPE geomembrane technological standard
NO Item standard
01 Thickness 0.2-3.0
02 Width 2.5-9.0
03 Tensile strength ≥14
04 Breaking elongation(%) ≥400
05 Rectangular tear strength(N/mm) ≥50
06 Permeability (g.cm/cm2.s.Pa) <1.0* 10 -13
07 Using temperature range +70~-70 Celsius Deg
Properties Test Value
0.75mm 1.00 mm 1.50 mm 2.00 mm
Thickness - mils (min. ave.)@ lowest individual of 10 values nom. (mil)-10% nom. (mil)-10% nom. (mil)-10% nom. (mil)-10%
Density (min.) 0.940 g/cc 0.940 g/cc 0.940 g/cc 0.940 g/cc
Tensile Properties (1) (min. ave.)@
yield strength@
break strength@
yield elongation@
break elongation
11 kN/m
20 kN/m
12%
700%
15 kN/m
27 kN/m
12%
700%
22 kN/m
40 kN/m
12%
700%
29 kN/m
53 kN/m
12%
700%
Tear Resistance (min. ave.) 93N 125 N 187 N 249 N
Puncture Resistance (min. ave.) 240N 320 N 480 N 640 N
Stress Crack Resistance (2) 300 hr. 300 hr. 300 hr. 300 hr.
Carbon Black Content - % 2.0-3.0% 2.0-3.0% 2.0-3.0% 2.0-3.0%
Carbon Black Dispersion note (4) note (4) note (4) note (4)
Oxidative Induction Time (OIT) (min. ave.) (5)
(a) Standard OIT_ or _
(b) High Pressure OIT
100 min.
400 min.
100 min.
400 min.
100 min.
400 min.
100 min.
400 min.
Oven Aging at 85°C (5), (6)
(a) Standard OIT (min. ave.) - % retained after 90 days_ or _
(b) High Pressure OIT (min. ave.) - % retained after 90 days
55%
80%
55%
80%
55%
80%
55%
80%
UV Resistance (7)
(a) Standard OIT (min. ave.)_ or _
(b) High Pressure OIT (min. ave.) - % retained after 1600 hrs
N.R. (8)
50%
N.R. (8)
50%
N.R. (8)
50%
N. R. (8)
50%

Contact us if you need more details on LDPE Geomembrane. We are ready to answer your questions on packaging, logistics, certification or any other aspects about HDPE Geomembrane、Geomembrane. If these products fail to match your need, please contact us and we would like to provide relevant information.