Find HDPE Geomembrane, PVC Geomembrane, LDPE Geomembrane on Industry Directory, Reliable Manufacturer/Supplier/Factory from China.

Inquiry Basket (0)
Home > Products > Geomembrane Welder > Colours Geomembrane blue, Green, Red with 0.15-3.0mm Thickness

Colours Geomembrane blue, Green, Red with 0.15-3.0mm Thickness

Payment Type: L/C, T/T, Western Union

Basic Info

Model No.:  hdpe geomembrane

Product Description

Model NO.: HDPE Geomembrane Surface: Smooth Feature: Puncture Resistance, Impact Resistance, Tear Resistance Color: According to The Customer Thickness: 0.15mm - 4.0mm Certificate: Ce/ISO9001, ISO1400, Ohsas18001 Trademark: RUNTONG Origin: Dezhou, China Certification: ISO Application: Transportation Project, Hydraulic Project, Geotechnical Project, Environmental Project Material: HDPE Width: Within 8 M (1m-8m). Optional Surface: Smooth or Textued(One or Two Side) Place of Origin: Dezhou, China Specification: ASTM HS Code: 3920109090 Colours Geomembrane Bule,Green ,Red with 0.15-3.0mm thickness 

Functions:
 Antiseep and separation
1. Prevent leakage disposal in landfill or waste water or waste dregs disposing field.
2. River bank, lake dam, mine remaining, reservoir, tunnel, liquid storage pool(pit, mine)
3. Preventing leakage in subway, basement, tunnel, hole. Anti-salt leakage in roadbed and other groundsill.
4. Used in Subgrade and other saline impervious Foundation.
5. The plane direction laying of dam, the vertical direction laying for groundsill, used in the construction fence and waste material field.
 Specification: Thickness 0.15-3.0mm
                      Length 50-200 or customized 
                      Width:1-8m
 Product Technological Standard:

 
NO Item Value
0.75mm 1.00mm 1.25mm 1.50mm 2.00mm 2.50mm 3.00mm
1 Density (g/cm 2 ) 0.939
2 Tensile propeties              
  Yield strength (N/mm) 11 15 18 22 29 37 44
  Break strength (N/mm) 20 27 33 40 53 67 80
  Yield elongation (%) 12
  Break elongation (%) ≥450
3 Tear resistance (N) 93 125 156 187 249 311 374
4 Puncture resistance (N) 240 320 400 480 640 800 960
5 Stree crack tensistance (h) ≥1500
6 Carbon black              
  Carbon black content (%) 2.0-3.0
  Carbon black dispersion Carbon black dispersion (only near spherical agglomerates)fo r10 different
  views 9 in categories 1 or 2 and 1 in category3  
7 Oxidative induction time(OIT)              
  Standard OIT(min) 100
  High pressure OIT(min) 400
8 Oven aging at 85 °C              
  Standard OIT-% retained after 90 days (%) 55
  High pressure OIT-% retained after 90 days (%) 80
9 UV Resistance              
  Standard OIT retained after 1600 hrs (%) 50
  High pressure OITretained after 1600 hrs (%) 50
10 Low tempreture impact brittle property at -70 °C Pass
11 Premeability ( g. cm/(cm 2 ). Pa) ≤ 1.0×10 -13
12 Dimensional stability (%) ±2

Contact us if you need more details on Geomembrane. We are ready to answer your questions on packaging, logistics, certification or any other aspects about HDPE Geomembrane、Waterproof Membrane. If these products fail to match your need, please contact us and we would like to provide relevant information.